2.30.
KEVLAR REPAIR continued
2.30.3. Small Cracks
a. Repair crack (1) in Kevlar fabric of less than 2
INCHES with edges remaining closed and
crack not extending through all laminations
(2).
(1) Stop drill (3) crack (1) at each end.
(2) Sand through crack (1) to an undamaged
lamination (4). Use paper (item 135, App F).
(3) Lightly sand away paint from area approxi-
mately 1.00 INCH around crack (1). Use
paper (item 135, App F).
b. Clean damaged area (para 1.47).